Baoji · Shaanxi · China  ·  ISO 9001:2015  ·  800+ t in stock
Materials — by grade Products — by form Industries Tools & calculators Technical guides News & notes Case deliveries About & factory Quality & certificates Contact / RFQ Request a quote
Home/Materials/Grade 5 · Ti-6Al-4V
Grade page · UNS R56400 · Ti-6Al-4V · TC4 · ВТ6

Grade 5 titanium (Ti-6Al-4V)

The workhorse alloy: alpha-beta, heat-treatable, roughly twice the strength of Gr2 at almost the same density. If your part is load-bearing, runs above 300 °C, or is thin-walled and being machined, this is the grade people specify — and the one most often specified wrongly.

Read this first: values below are typical mill values for the forms we supply. Density is not a specification requirement and is not a guaranteed value. Always verify suitability against the governing specification on your drawing — ASTM B265, B348, B367, B861 and F136 control different things.

Chemical composition

Per ASTM B348 / B265, mass %. These are range limits, not targets.

ElementMin %Max %Why it matters
Aluminium5.506.75Alpha stabiliser — strength and oxidation resistance
Vanadium3.504.50Beta stabiliser — ductility and hardenability
Iron—0.30Excess iron embrittles; a common cheap-heat tell
Oxygen—0.25Raises strength, cuts ductility and machinability
Carbon—0.08Interstitial strengthener; watch on repeat heats
Nitrogen—0.05Small effect, tightly held
Hydrogen—0.015Hydride risk if it climbs
Titanium—bal.Remainder

Gr23 (ELI) is the same alloy with oxygen capped at 0.13 % and iron at 0.25 %. That difference is the entire reason it behaves better in thin machined sections.

Mechanical properties — as supplied

PropertyMetricImperialMethodCondition
Tensile strength, UTS≥ 895 MPa≥ 130 ksiASTM E8Mill annealed
Yield strength, Rp0.2828 MPa typ.120 ksiASTM E8Mill annealed
Elongation A10 %10 %ASTM E8Mill annealed
Reduction of area30 %30 %ASTM E8Mill annealed
Hardness364 HB typ.≈ 38 HRCASTM E10Mill annealed
Modulus of elasticity110 GPa16 MsiASTM E111Room temperature
Fatigue strength (10⁷ cycles)≈ 483 MPa70 ksiASTM E466Smooth bar, R = −1
Fracture toughness KIC66 MPa·m½60 ksi·in½ASTM E399Aged plate

Physical & thermal

DensityMelting rangeβ transusThermal cond.Specific heatCTE 20–200 °CResistivity
4.43 g/cm³
0.160 lb/in³
1604–1660 °C≈ 995 °C6.7 W/m·K526 J/kg·K8.6 µm/m·K170 µΩ·cm

Standards by product form

Same grade, different specification depending on what you are buying. This is where most mis-quotes start.

FormASTM / ASMEDIN / ENGBGOSTAerospace
Plate & sheetB265 Gr53.7164 / TA6VGB/T 3621 TC4ВТ6AMS 4911
Seamless tubeB337 Gr53.7034GB/T 3625ВТ6AMS 4928
Welded tubeB338—GB/T 3625—AMS 4929
Bar, billet, forgingsB348 Gr53.7164GB/T 2965ВТ6AMS 4928 / 4965
WireB863 Gr5—GB/T 3629—AMS 4919
FittingsB367 Gr2 (Ti-6Al-4V)—GB/T 13678—ASME B16.9
FlangesB381 F5—NB/T 47010—ASME B16.5
FastenersF1341DIN 6923 (mat.)GB/T 3099.1—NAS 1803 / MS21245
Where two specs disagree: B381 flange grade F5 maps to Ti-6Al-4V, but F2 maps to CP Gr2. Buyers routinely order “Gr5 flange to B16.5” and receive an F2 facing. Name the B381 grade, not just the words “Grade 5”.

Equivalent designations

UNSTrade / regionalChineseRussianEuropeanJapanese
R56400Ti-6Al-4V · Timetal 6-4 · VST5-1TC4 / TA6VВТ6 (VT6)3.7164 / TA6VTi-6Al-4V (JIS H 4603)

Equivalence is by composition and strength class, not by guaranteed performance. Verify against the governing specification for your application.

What we hold right now

Form / gradeSizeStandardOn floorFOB USD/kgShip within
Gr5 (TC4) bar Ø60 mm drawn ASTM B348 41 t 12.40 7 days

Stock figures refreshed 2026-11-01. Blank cells mean we do not hold that form — ask and we will quote a rolling slot instead.

Selection traps we see every month

选型陷阱条目

1 · Gr5 for a thin-walled machined part

Gr5 is harder to cut and less forgiving at small sections than Gr23. If you are CNC-ing something under about 6 mm wall, run the tool-life maths before you commit — the ELI premium usually pays for itself in one avoided scrapped batch.

2 · Assuming “Grade 5” settles the corrosion story

Alloying for strength costs a little corrosion margin versus CP grades. In hot chloride or reducing-acid service, Gr7 or Gr2 is often the cheaper answer over the asset's life, even though the per-kg price looks worse.

3 · Specifying heat treatment on the PO but not the drawing

Mill-annealed and solution-treated-plus-aged give very different numbers from the same heat. If your PO says “895 MPa min” without a condition, we will quote mill annealed and you may receive a part that fails a proof test.

FAQ

Yes in composition and strength class. TC4 is the Chinese GB designation; both map to UNS R56400. What is not the same is the tolerance band and the test set required by GB/T 2965 versus ASTM B348.

Yes, but tell us before we machine. Solution treating plus ageing distorts thin sections, and a finished ±0.02 mm bearing journal will not survive it without a straightening pass.

For implant duty specify Gr23 / F136 or F67, not Gr5. We supply ELI bar with per-heat traceability, and we will not substitute Gr5 for a F136 requirement.

500 kg from stock, cut to length. Below that, shearing setup makes the unit price unreasonable.


相关内容

Related product

Gr5 / TC4 plate 10 mm

22 t on floor · FOB 13.10 · ships in 7 days

Open datasheet →
Related guide

Gr5 vs Gr23 for machined parts

Where the line falls, with tool-life maths

Read →
Related tool

Weight calculator (Gr5 preset)

4.43 g/cm³, formula shown on screen